unleash1Jun 15, 20191 min readA Wiengmoon, T. Chairuangsri and J.T.H. Pearce. “Effects of Heat Treatment on Microstructure and Properties of 20wt%Cr and 27wt%Cr White Cast Irons”. Netsu Shori, Journal of the Japan Society for Heat Treatment (2009) Vol.49 October pp.510-513.
“Effects of Heat Treatment on Microstructure and Properties of 20wt%Cr and 27wt%Cr White Cast Irons”. Netsu Shori, Journal of the Japan Society for Heat Treatment (2009) Vol.49 October pp.510-513.
J.T.H. Pearce.“Heat Treatment of Aluminium Castings”. Metal Casting Technologies (2002) Vol.48 No.2 June pp.40-43.
J.T.H. Pearce.“High Chromium Cast Irons to Resist Abrasive Wear”. The Foundryman (2002) Vol.95 April pp.156-166.
P. Niranatlumpong, J.T.H. Pearce et Al.,“Wear: Principles and Prevention”. MTEC Monograph (2002), Bangkok, Thailand, 148pp. ISBN 974 229 252 3.[In Thai]