unleash1Jun 15, 20191 min readRabbani, F., Ward, L.P., Strafford, K.N. and Netting, A ; A Comparison of the Growth Kinetics and Scale Morphology for Three Superalloys at 930 °C in Air and Low pO2 Environments. Oxidation of Metals 54 (1 – 2) (2000) 139 - 153
A Comparison of the Growth Kinetics and Scale Morphology for Three Superalloys at 930 °C in Air and Low pO2 Environments. Oxidation of Metals 54 (1 – 2) (2000) 139 - 153
J.T.H. Pearce.“Heat Treatment of Aluminium Castings”. Metal Casting Technologies (2002) Vol.48 No.2 June pp.40-43.
J.T.H. Pearce.“High Chromium Cast Irons to Resist Abrasive Wear”. The Foundryman (2002) Vol.95 April pp.156-166.
P. Niranatlumpong, J.T.H. Pearce et Al.,“Wear: Principles and Prevention”. MTEC Monograph (2002), Bangkok, Thailand, 148pp. ISBN 974 229 252 3.[In Thai]